PITTING & CORROSION PREVENTING ANODES

Zinc Hull Anodes

Zinc marine anodes from Thermal are manufactured from Special High Grade Zinc, 99.995% pure, the highest grade of zinc available. Our customized blending system provides even distribution throughout of all critical additives required to meet Military Specification – MIL-A-18001J. This careful attention to alloying and casting procedures results in a full line of products that provides maximum long life protection for steel in seawater and saline mud.In addition, Thermal fills custom orders to your exact specifications. With on-time delivery in any quantity.

Cat. No. TRC-48 / TRC-26 / TRR-23 / TRC-42 / TRC-23B / TRC-23C / TRC-12C / TRC-23T / TRC-11-W / TRC-12 / TRC-24 / TRC-6-W / TRC-TD6 / TRC-5C

SKU: N/A Category:

Description

 

Cat. No.SizeCurrent Amp-Yr. RatingMethod ofNo. of Cast-in Galvanized Steel StrapsType
TRC-484 1/2” x 24” x 2 1/4”2Welding1*
TRC-264 1/4” x 14” x 2 1/4”1Welding or Bolting1*
TRC-236” x 12” x 1 1/4”1Welding2*ZHS-23
TRC-426” x 12” x 2 1/2”1Welding2ZHS-42
TRC-23B6” x 12” x 1 1/4”1Welding2***ZHB-23
TRC-23C6” x 12” x 1 1/4”1Bolting1ZHC-23
TRC-123” x 12” x 1 1/4”1/2Bolting1
TRC-23T TAPERED6 1/2” X 14” X 1 1/4”1Welding2*
TRC-11-W6” x 6” x 1 1/4”1/2Welding1
TRC-123” x 12” x 1 1/4”1/2Welding1*ZSS-12
TRC-243 1/2” x 12” x 2 1/2” “1/2Welding1*ZSS-24
TRC-6-W3” x 6” x 1 1/4” “Welding1*
TRC-TD6 TEAR DROP3” x 9” x 1 1/4” “1/4Welding or Bolting1*ZTS
TRC-5C2 1/2” x 9” x 1 1/2” “1/4Bolting1

* Strap holes optional
** Also available in 3-section plate
*** Phosphor Bronze Strap

HULL TYPE ANODES
AluminumZincMagnesium
Indium – Activated ACS 4Mil*A*180001 (latest rev.)Grade H – 1
Mil. No.Wt.WLHMil. No.Wt.WLHPart No.Wt.WLH
AHS-1096121.25ZHS-23 (M – 24)226121.25H-6 C66121.25
AHC-1096121.25ZHC-26 (N-23 C)216121.25H-11116122.50
AHS-20176122.50ZHS-42 (M-42)416122.50H-11 C116122.50
AHC-20166122.50ZHC-42 (M-42 C)396122.50H-24249182
These anodes are equipped with two cast – in mounting straps or two cast – in cored holes on 6” centers.H-44449184
AluminumZincMagnesium
Indium Activated ACS4Mil*A*180001 (latest rev.)Grade H -1
Mil. No.Wt.WLHMil. No.Wt.WLHPart No.Wt.WLH
ASS-553121.25ZSS-12 (M-12)113121.25H-333121.25
ASS-1093122.50ZSS-24 (M-22)223122.50H-6 L63122.50
These anodes are equipped with a single cast – in mounting strap.
AluminumZincMagnesium
Indium Activated ACS4Mil*A*180001 (latest rev.)Grade H -1
Mil. Spec.Wt.WLHMil. Spec.Wt.WLHPart No.Wt.WLH
STS2391.38ZTS (M-6)5391.38H-11.25391.38
ATS-44392.50ZTS-1010392.50H-2.52.5392.50
ATS85102.50ZTS-20205102.50H-555102.50
A tear drop shaped anode equipped with a single cast – in mounting strap.
AluminumZincMagnesium
Indium Activated ACS4Mil*A*180001 (latest rev.)Grade H-1
Part No.Wt.WLHPart No.Wt.WLHPart No.Wt.WLH
ACS-12124142.25LL.-26264142.25H-884142.25
ACS-20204242.25LL.-48484242.25H-13134242.25
ACS-23235242.00LL.-58585242.00H-15155242.00
ACS-29295242.50LL.-73735242.25H-18185242.50
Includes single longitudinal mounting strap.

Notes: 1. Zinc and magnesium anode strap core are galvanized, brass straps available for zinc anodes.
2. All magnesium anodes available with plastisol coating.
3. Other alloys available: aluminum, tin, mercury activated; Mil-A-24779 (S H); zinc – high purity; magnesium – high potential.
4. Other core configurations available.